Zeolite process for water softening
What is zeolite
Zeolite is micro-porous mineral which is used as catalyst in many industrial
purposes such as water purification and air purification. The zeolites are
hydrated aluminosilicates and general composition AlxSiyO2(x+y) (without
water molecules). Zeolites are two types natural and synthetic or artificial.
The natural zeolite that is used for water softening is gluconites or
greensand. Permutit is the synthetic zeolite that is most used in water
softening and its chemical formula is Na2O, Al2O3,
nSiO2, xH2O. These are used as ion exchanger and odor
removal in water softener. Permutit are more porous, glassy, and have higher
softening capacity than greensand. Zeolites are characteristically soft to
moderately hard, light in density, insoluble in water but can act as base
exchangers in contact with water containing cations. Hence these can remove Ca2+ and
Mg2+ ions from water when hard water is passes through. Newstone’s
100% Natural Zeolite Rock – 5mm to 10mm Small Natural Zeolite Rock , Mined From
Japan (1.1lbs / 500grams) – Great for Odor Removal in Room, Use in Aquarium to
Remove Ammonium or Odor Eater
Zeolite process for water softening
Zeolite
process for water softening has become a commercial success for the reason that
zeolite can be easily regenerated. When Ca2+ and Mg2+ ions
containing hard water is passes through a bed of sodium zeolite, the sodium
ions are replace by the calcium and magnesium ions.
Na2Ze
+ Ca(HCO3)2 → 2NaHCO3 +
CaZe
Na2Ze + Mg(HCO3)2 → 2NaHCO3 +
MgZe
Na2Ze + CaSO4 → Na2SO4 +
CaZe
Na2Ze + MgSO4 → Na2SO4 +
MgZe
When all sodium ions are replaced by calcium and magnesium ions, the zeolite becomes inactive. Then the zeolite needs to be regenerated. Brine solutions are passing through the bed of inactivated zeolite. The following reactions are taken place and form Na2Ze.
CaZe
+ 2NaCl → Na2Ze + CaCl2
MgZe + 2NaCl → Na2Ze + MgCl2
The
softening water by this process is used for laundry process and cannot be used
for boiler purpose. Because this water softening system contains NaHCO3 in
the water; when this water is heated, it produces CO2 which is
corrosive for boilerplates.